Table 4 Comparison of EPO and Eeff from the 1st indentation cycle

From: Mechanism and Method of Testing Fracture Toughness and Impact Absorbed Energy of Ductile Metals by Spherical Indentation Tests

Material

ET (GPa)

EPO (GPa)

\(\frac{{E_{{{\text{PO}}}} - E_{{\text{T}}} }}{{E_{{\text{T}}} }}\)

(%)

Eeff (GPa)

\(\frac{{E_{{{\text{eff}}}} - E_{{\text{T}}} }}{{E_{{\text{T}}} }}\)

(%)

Q345R

190

118

–37.9

180

–5.2

SA508-3

206

144

–30.1

199

–3.4

18Mn

195

132

–32.3

200

2.6

S30408

173

127

26.5

182

5.2