Skip to main content

Table 4 EDS results of site A-J in Figure 9 (wt%)

From: Fretting Wear Characteristics of Nuclear Fuel Cladding in High-Temperature Pressurized Water

Element

B

C

D

E

F

G

H

O

2.89

9.20

10.41

6.96

11.85

11.39

14.07

Fe

0.09

0.22

0.39

0.28

0.26

0.28

0.39

Zr

94.66

88.63

86.63

79.19

77.31

80.37

76.24

Nb

1.08

0.85

1.48

12.93

9.75

6.82

8.79

Sn

1.28

1.11

1.09

0.65

0.84

1.14

0.52