Fig. 5From: Defect Formation Mechanisms in Selective Laser Melting: A ReviewSEM images of crack morphology and microstructure from the cross section of an SLM fabricated Ti6Al4V part: (a) crack morphology; (b) microstructure on both sides of the crack [40]Back to article page