Fig. 8From: Defect Formation Mechanisms in Selective Laser Melting: A ReviewOptical images of defect morphologies at different energy inputs in the SLM-processed Ti6Al4V parts: (a) spherical porosities (P = 120 W, v = 40 mm/s); (b) incomplete fusion holes (P = 120 W, v = 1500 mm/s) [47]Back to article page