From: Defect Formation Mechanisms in Selective Laser Melting: A Review
Location
1
2
3
4
O
0.87
41.75
2.55
0.4
Mg
0.30
0.58
0.31
0.26
Al
88.57
56.42
86.96
88.17
Si
10.24
1.23
10.20
11.18
Total
100.00