Figure 9From: Structure of Micro-nano WC-10Co4Cr Coating and Cavitation Erosion Resistance in NaCl SolutionCrater micrographs of WC-10Co4Cr coatings after 16 h cavitation erosion in 3.5 wt % NaCl solution. (a) MC, (b) CC, (c) CCBack to article page