Skip to main content

Table 3 Porosity, microhardness and fracture toughness of WC-10Co4Cr coatings

From: Structure of Micro-nano WC-10Co4Cr Coating and Cavitation Erosion Resistance in NaCl Solution

Specimen

Porosity

/ %

Microhardness

HV/MPa

Fracture toughness

K c /(MPa·m1/2)

MC

0.26 ± 0.07

1345 ± 136

5.58 ± 0.50

CC

0.43 ± 0.12

1322 ± 181

3.83 ± 0.52