Figure 5From: Effect of Trace Addition of Ceramic on Microstructure Development and Mechanical Properties of Selective Laser Melted AlSi10Mg AlloyMorphologies of the molten pool on cross sections of SLM-processed TiB2/AlSi10Mg composite samples at different parameters (P = 400 W): av = 2000 mm/s; bv = 2400 mm/s; cv = 2800 mm/s; dv = 3200 mm/sBack to article page