Table 1 Electrolyte composition and electrolysis conditions

From: Preparation of Nickel-Cobalt/Carborundum Carbide Composite Coatings by Supergravity Field-Enhanced Electrodeposition

Component Concentration
Nickel sulphamate (g/L) 350
Nickel chloride (g/L) 15
Boric acid (g/L) 35
Cobalt sulphamate (g/L) 40
SiC (g/L) 2
Electrolyte temperature (°C) 45 ± 1
Current density (A/dm2) 2
Rotation speed (r/min) 0, 400, 800, 1200, 1600