From: Face Grinding Surface Quality of High Volume Fraction SiCp/Al Composite Materials
No. | Spindle speed (r/min) | Feeding amount (mm/min) | Grinding depth (μm) |
---|---|---|---|
T1 | 2000 | 50 | 5 |
T2 | 2000 | 50 | 20 |
T3 | 2000 | 50 | 40 |
T4 | 2000 | 50 | 80 |
T5 | 4000 | 50 | 5 |
T6 | 4000 | 50 | 20 |
T7 | 4000 | 50 | 40 |
T8 | 4000 | 50 | 80 |
T9 | 6000 | 50 | 5 |
T10 | 6000 | 50 | 20 |
T11 | 6000 | 50 | 40 |
T12 | 6000 | 50 | 80 |
T13 | 8000 | 50 | 5 |
T14 | 8000 | 50 | 20 |
T15 | 8000 | 50 | 40 |
T16 | 8000 | 50 | 80 |
T17 | 2000 | 100 | 5 |
T18 | 2000 | 100 | 20 |
T19 | 2000 | 100 | 40 |
T20 | 2000 | 100 | 80 |
T21 | 4000 | 100 | 5 |
T22 | 4000 | 100 | 20 |
T23 | 4000 | 100 | 40 |
T24 | 4000 | 100 | 80 |
T25 | 6000 | 100 | 5 |
T26 | 6000 | 100 | 20 |
T27 | 6000 | 100 | 40 |
T28 | 6000 | 100 | 80 |
T29 | 8000 | 100 | 5 |
T30 | 8000 | 100 | 20 |
T31 | 8000 | 100 | 40 |
T32 | 8000 | 100 | 80 |