Table 4 Experimental parameters comparison of T9 and T10

From: Face Grinding Surface Quality of High Volume Fraction SiCp/Al Composite Materials

No.

T9

T10

Feeding amount (mm/min)

50

50

Grinding depth (μm)

5

20

Spindle speed (r/min)

6000

6000

F

0.80

2.10

COF

0.29

0.30

Sdr

1.06

1.02

Ra

2.08

2.59

Rab

0.26

0.31

Rp

14.39

16.29

Rv

18.59

18.55

Ssk

−0.11

−0.69

Sku

3.68

4.05