Skip to main content

Table 7 Experimental parameters comparison of T27 and T28

From: Face Grinding Surface Quality of High Volume Fraction SiCp/Al Composite Materials

Parameter

T27

T28

Feeding amount (mm/min)

50

50

Grinding depth (μm)

40

80

Spindle speed (r/min)

6000

6000

F

3.50

6.5

COF

0.36

0.38

Sdr

1.19

1.24

Ra

3.03

3.61

Rab

0.19

0.22

Rp

19.62

19.69

Rv

22.70

20.60

Ssk

−0.30

−0.03

Sku

2.91

2.26