Figure 6From: Variation in Deformation Behaviors Along the Transverse Direction During the Warm Rolling of a 1480-mm-Wide AZ31B PlateTrue stress–true strain curves of different regions at a strain rate of 15 s−1 and at (a) 220 °C and (b) 270 °CBack to article page