Figure 19From: A Review on Friction Stir Welding of SteelsPrecipitate distributions of the stir zone (SZ) at different conditions: a SZ in the as-welded, b SZ tempered at 720 °C, c SZ tempered at 760 °C, d SZ tempered at 800 °C [180]Back to article page