Table 1 SLM process parameters

From: Microstructures, Thermal and Mechanical Properties of Pure Tungsten—A Comparison Between Selective Laser Melting and Hot Rolling

Laser power (W) Scan speed (mm/s) Hatch spacing (μm) Layer thickness (μm)
200 200 100 30