Skip to main content

Table 3 Factors and levels of Taguchi experimental

From: Microstructure, Properties and Crack Suppression Mechanism of High-speed Steel Fabricated by Selective Laser Melting at Different Process Parameters

Factors

Levels

Laser power

P(W)

Scan speed

v(mm/s)

Scan distance

h(mm)

Substrate temperature

T(℃)

1

180

870

0.06

50

2

200

960

0.07

100

3

220

1050

0.08

150

4

240

1140

0.09

200