Skip to main content

Table 4 Identified parameters in the Hill48 yield function

From: Investigation on Yield Behavior of 7075-T6 Aluminum Alloy at Elevated Temperatures

Temp.
(°C)
F G H N
25 0.3491 0.6146 0.3854 1.2644
130 0.3492 0.6131 0.3869 1.2481
180 0.3678 0.6064 0.3936 1.3045
230 0.4639 0.6039 0.3961 1.403