Figure 4From: Friction-Induced Nanofabrication: A ReviewAFM images (top) and cross-sectional profiles (bottom) of the scratches on Si(100) surface after line-scratching under various normal load Fn [36] (The diamond tip for the test has tip radius of about 0.15 μm, D = 100 nm and N = 100)Back to article page