Table 4 Maximum Mises stress of the upper and lower plates under loads of mean fatigue limit P50

From: Fatigue Resistance and Failure Behavior of Penetration and Non-Penetration Laser Welded Lap Joints

Specimen P50 (kN) Upper plate σMises Lower plate σMises
0.8+1.5-N 3.47 387 326
1.5+0.8-P 4.34 354 408