Table 3 EDX quantification results (wt%) indicated in Figure 6b

From: Refill Friction Stir Spot Welding Al Alloy to Copper via Pure Metallurgical Joining Mechanism

Location Mg Al Cu Table
1 0.6 94.3 5.1 100.0
2 0.6 93.8 5.6 100.0