From: Influence of Ultrasonic Surface Rolling Process and Shot Peening on Fretting Fatigue Performance of Ti-6Al-4V
\({\sigma }_{b}\) (MPa)
\({\sigma }_{0.2}\) (MPa)
\(E\) (GPa)
Elongation after fracture (%)
\(\mu \)
820
740
120
11
0.34