Wire-based laser cladding layers of Ti-6Al-4V in (a) underwater and (b) in-air environment [41]; Cross sections of the single track Ti-6Al-4V deposited in underwater and in air environments: (c) 10 L/min, (d) 18 L/min, (e) 20 L/min, (f) in-air environment [42]