Figure 5From: Research Progress of Refractory High Entropy Alloys: A ReviewSEM backscattered electron images of the bulk NbMoTaWVCr HEA alloys sintered at different temperatures: (a) 1400, (b) 1500, (c) 1600 and (d) 1700 [37]Back to article page