Skip to main content

Table 2 Tensile Properties of SLM-Fabricated Ti6Al4V Alloys and Wrought Counterpart

From: Defect Formation Mechanisms in Selective Laser Melting: A Review

Process Yield strength (MPa) Ultimate tensile strength (MPa) Elongation (%)
SLM [17] 1110 1267 7.28
SLM [24] 1137 1267 7.28
SLM [51] 1125 1250 6
SLM [62] 1075 1199 7.6
SLM [63] 1008 1080 1.6
SLM [64] 990 1095 8.1
Wrought [65] 922 984 19.3